AL--Nonwoven Oven Waste Felt Non Woven Making Machine
1.Final Products Name:waste felt oven nonwoven fabric making machine
2.Raw Material:Polyester staple fiber, polyester hollow staplefiber (optional),Low melting point fiber and natural wool fiber etc, specification:4D-25D
3.Production process: A percentage of polyester staple fiber ,hollow staple polyester( waste fiber or waste cloth fiber) and low melting point fibers be opened and blended by opener, then carded and lapped with required thickness, and set by the process of needle , oven and setting.
4.Products feature: good permeability, good warmth retention property, lightweight sound absorbing, high resilience, anti-aging, washable, clean with no harmful substances.
5.Raw Material Ratio: Usually low melting point fiber 4Dx51mm 15%-25%, hollow polyester staple 6DX51-65mm 40-50%(optional), Polyester fiber 6DX51-65mm 30-40%;
Production Line technical parameters
1.Machine Width: 2000mm---3500mm
2.Thickness:10~120mm
3.Product GSM:100~5000g/m2
4.Product Capacity:100~500kg/h (according to product specification)
5.Oven Temperature: ≤230℃
6.Heating Method: gas
7.Production Line Processing :
Bale Opener→Main opening→Big Cabinet Blender →Vibrating Feeder→Single Cylinder Carding Machine→Cross Lapper→Drying and Setting Oven→Cooling Machine→Automatic Slitter and Winder
AL--Nonwoven Oven Waste Felt Non Woven Making Machine
1.Final Products Name:waste felt oven nonwoven fabric making machine
2.Raw Material:Polyester staple fiber, polyester hollow staplefiber (optional),Low melting point fiber and natural wool fiber etc, specification:4D-25D
3.Production process: A percentage of polyester staple fiber ,hollow staple polyester( waste fiber or waste cloth fiber) and low melting point fibers be opened and blended by opener, then carded and lapped with required thickness, and set by the process of needle , oven and setting.
4.Products feature: good permeability, good warmth retention property, lightweight sound absorbing, high resilience, anti-aging, washable, clean with no harmful substances.
5.Raw Material Ratio: Usually low melting point fiber 4Dx51mm 15%-25%, hollow polyester staple 6DX51-65mm 40-50%(optional), Polyester fiber 6DX51-65mm 30-40%;
Production Line technical parameters
1.Machine Width: 2000mm---3500mm
2.Thickness:10~120mm
3.Product GSM:100~5000g/m2
4.Product Capacity:100~500kg/h (according to product specification)
5.Oven Temperature: ≤230℃
6.Heating Method: gas
7.Production Line Processing :
Bale Opener→Main opening→Big Cabinet Blender →Vibrating Feeder→Single Cylinder Carding Machine→Cross Lapper→Drying and Setting Oven→Cooling Machine→Automatic Slitter and Winder